California Fine Wire Alloy 52 Nickel Iron Alloy

Category Metal , Ferrous Metal , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Alloy 52 Nickel Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.25 g/cc
0.298 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 483 MPa
70000 psi
Annealed
896 MPa
130000 psi
Stress relieved
1030 MPa
150000 psi
Hard
Tensile Strength, Yield 276 MPa
40000 psi
Annealed
552 MPa
80000 psi
Stress relieved
689 MPa
100000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 9.80 µm/m-°C

@Temperature 20.0 °C
5.44 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 20.0 °C
0.115 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 13.2 W/m-K
91.6 BTU-in/hr-ft²-°F
Melting Point 1430 °C
2600 °F
Component Elements Properties Metric English Comments
Iron, Fe 50 %
50 %
Nickel, Ni 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000429 ohm-cm
0.0000429 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0035 ohms/ohm-°C
0-100°C