Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.90 µm/m-°C @Temperature 23.0 - 260 °C |
2.72 µin/in-°F @Temperature 73.4 - 500 °F |
ASTM D696 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
CTE, linear | 4.90 µm/m-°C | 2.72 µin/in-°F | at Set Pt. |
Ferro EG 2807 Metal Sealing Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 260 °C |
2.72 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2807 Metal Sealing Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 300 °C |
2.72 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott FIOLAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Pharmaceutical primary packagingInformation provided by SCHOTT AG. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 1000 °C |
2.72 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ceralloy® 1370-1E Aluminum Nitride Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 27.0 - 175 °C |
2.72 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7951 Hi-Performance Acrylic 300MP This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app.. |
|||
CTE, linear | 4.90 - 5.70 µm/m-°C | 2.72 - 3.17 µin/in-°F | |
CeramTec Ceramtape GC Glass Ceramic LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |
|||
CTE, linear | 4.90 µm/m-°C @Temperature 20.0 - 300 °C |
2.72 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott DUROBAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is.. |