Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.90 - 5.70 µm/m-°C | 2.72 - 3.17 µin/in-°F | |
CeramTec Ceramtape GC Glass Ceramic LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |