Polymer Property : CTE, linear = 38.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 34.1 - 38.3 µm/m-°C

@Temperature -60.0 - 60.0 °C
18.9 - 21.3 µin/in-°F

@Temperature -76.0 - 140 °F
Mateck Potassium Chloride (KCl)
Optical crystals