Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 34.1 - 38.3 µm/m-°C @Temperature -60.0 - 60.0 °C |
18.9 - 21.3 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Potassium Chloride (KCl) Optical crystals |