Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 224 µm/m-°C | 124 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |