Thermal Properties Metric English Comments
CTE, linear 224 µm/m-°C
124 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, ..