Thermal Properties Metric English Comments
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 2241 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio..
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide
Single-part castable ceramic exhibiting high strength and thermal conductivity.
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride
Fine grain aluminum nitride castable with high thermal conductivity
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride
Fine grain aluminum nitride castable with high thermal conductivity.