Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.250 µm/m-°C @Temperature <=1010 °C |
0.139 µin/in-°F @Temperature <=1850 °F |
|
Pyrotek Pyrocast ICL Castable Refractory Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist.. |
|||
CTE, linear | 0.250 µm/m-°C @Temperature <=1010 °C |
0.139 µin/in-°F @Temperature <=1850 °F |
|
Pyrotek Pyrocast TG Castable Refractory Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel.. |