Pyrotek Pyrocast TG Castable Refractory

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast TG Castable Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel-type furnace lining Kilns Boilers Heat treating furnaces Forge furnaces Copper base alloys AdvantagesExcellent thermal shock resistance Dimensionally stable Good insulation for density Does not inhibit induction energy transfer Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.875 g/cc
0.06774 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00800 GPa

@Temperature 850 °C
1.16 ksi

@Temperature 1560 °F
Compressive Strength 38.0 MPa

@Temperature 850 °C
5510 psi

@Temperature 1560 °F
Thermal Properties Metric English Comments
CTE, linear 0.250 µm/m-°C

@Temperature <=1010 °C
0.139 µin/in-°F

@Temperature <=1850 °F
Thermal Conductivity 0.600 W/m-K

@Temperature 540 °C
4.16 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.610 W/m-K

@Temperature 295 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 563 °F
0.780 W/m-K

@Temperature 815 °C
5.41 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Maximum Service Temperature, Air 1480 °C
2700 °F
Shrinkage 0.200 %

@Temperature 1090 °C
0.200 %

@Temperature 1990 °F
Component Elements Properties Metric English Comments
Al2O3 16 %
16 %
CaO 6.0 %
6.0 %
Other 4.0 %
4.0 %
SiC 74 %
74 %