Material Notes:
Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resistance.ApplicationsInduction coil liningBoiler preheater liningComponent liningsAdvantagesExcellent window for induction energyExtremely stableThermal shock resistantMinimum maintenanceResilient to crackingFewest shortsLong-life coil lining Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0100 GPa
1.45 ksi
Compressive Strength 41.0 MPa
5950 psi
Thermal Properties Metric English Comments
CTE, linear 0.250 µm/m-°C

@Temperature <=1010 °C
0.139 µin/in-°F

@Temperature <=1850 °F
Thermal Conductivity 0.620 W/m-K

@Temperature 295 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 563 °F
0.690 W/m-K

@Temperature 540 °C
4.79 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.820 W/m-K

@Temperature 815 °C
5.69 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage 0.200 %

@Temperature 1090 °C
0.200 %

@Temperature 1990 °F
Component Elements Properties Metric English Comments
Al2O3 19 %
19 %
CaO 6.0 %
6.0 %
Other 1.0 %
1.0 %
SiC 74 %
74 %