Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 45 mm/min | 1.8 in/min | SAE J 369 |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Flame Spread | 45 mm/min | 1.8 in/min | Horizontal Burning Speed 2mm thickness; ISO 3795 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Flame Spread | 46 mm/min @Thickness 1.00 mm |
1.8 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i.. |
|||
Flame Spread | 46 mm/min | 1.8 in/min | burn rate |
AlphaGary Evoprene™ LF 6152 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Flame Spread | 45 mm/min | 1.8 in/min | burn rate |
AlphaGary Evoprene™ LF 6153 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |