DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced, Impact Grade
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods include injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
ISO 294-4 2577
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
ISO 527-1/-2
Elongation at Break 37 %
37 %
Nominal; ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-1/-2
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1/-2
Flame Spread 46 mm/min

@Thickness 1.00 mm
1.8 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Emissions <2 mg/kg
VDA 275
Part Marking Code >POM-I<
ISO 11469
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-I
ISO 1043