Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa PC QUINN PC sheets have excellent optical properties and a brilliant surface. The QUINN PC range contains sheets that are easy to fabricate and show exceptional performance at both low and high tempera.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa COPOL PETG QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Decomposition Temperature | >= 280 °C | >= 536 °F | |
Polycasa SAN QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional s.. |