Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 29.0 °C | 84.2 °F | |
KiON HTT 1800 General DescriptionKiON HTT 1800 is a pale yellow, low viscosity liquid polysilazane-based coating resin that is specially designed for use in the formulation of heat-curable ceramic coatings capabl.. |
|||
Flash Point | 29.0 °C | 84.2 °F | Seta |
Lord Adhesives Flocklok® 852 Flock Adhesive LORD Flocklok® 852 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res.. |
|||
Flash Point | 29.0 °C | 84.2 °F | Curative 44; Seta |
Lord Adhesives Chemlok® 485/Curative 44 Adhesive LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers.. |
|||
Flash Point | 29.0 °C | 84.2 °F | closed cup |
Dow Corning Z-6124 SILANE Dow Corning® Z-6124 Silane has the chemical formula: (CH3O)3Si and is designated phenyltrimethoxy silane. Dow Corning Z-6124 Silane is a chemical monomer that reacts with water to form a silanetrio.. |