Material Notes:
LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers (TPEs).All information provided by Lord.
Physical Properties Metric English Comments
Density 0.850 - 0.8747 g/cc
0.0307 - 0.03160 lb/in³
Chemlok® 485
1.02 - 1.04 g/cc
0.0368 - 0.0377 lb/in³
Curative 44
Solids Content 15 - 17 %
15 - 17 %
Chemlok® 485
47 - 51.5 %
47 - 51.5 %
Curative 44
Brookfield Viscosity <= 10 cP

@Temperature 25.0 °C
<= 10 cP

@Temperature 77.0 °F
Curative 44; LVT, Spindle #2 @ 30rpm
400 - 1000 cP

@Temperature 25.0 °C
400 - 1000 cP

@Temperature 77.0 °F
Chemlok® 485; LVT, Spindle #2 @ 30rpm
Thermal Properties Metric English Comments
Flash Point -4.00 °C
24.8 °F
Chemlok® 485; Seta
29.0 °C
84.2 °F
Curative 44; Seta
Processing Properties Metric English Comments
Dry Time 0.5 - 1 hour
0.5 - 1 hour
24 hour

@Temperature 23.0 °C
24 hour

@Temperature 73.4 °F
Full bond strength
Shelf Life 12.0 Month

@Temperature 21.0 - 27.0 °C
12.0 Month

@Temperature 69.8 - 80.6 °F
Descriptive Properties Value Comments
Appearance Clear to Amber Liquid
485
Transparent Brown Liquid
Curative 44
Solvents MEK, Xylene
Xylene
Copyright © lookpolymers.com All Rights Reserved