KiON HTT 1800

Category Fluid , Polymer , Thermoset
Manufacturer KiON, A Clariant Business
Trade Name HTT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KiON HTT 1800.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionKiON HTT 1800 is a pale yellow, low viscosity liquid polysilazane-based coating resin that is specially designed for use in the formulation of heat-curable ceramic coatings capable of withstanding operating temperatures of 1800°F or above. KiON HTT 1800 is supplied as a 100% “solids” liquid of low viscosity, and rapidly solidifies upon heating to 350-400°F. KiON HTT 1800 can be blended with a variety of pigments, such as metal powders (zinc, aluminum, stainless steel), ceramic powders (silicon carbide, aluminum oxide, silicon nitride), or the like. For ultra-high temperature formulations, the coated part is then heated to at least 850°F to promote conversion of the polymer to ceramic. Depending on the exact formulation, coating operating temperatures of 1800°F or above can be achieved.ApplicationsHigh Temperature Coatings and Thermally Stable Corrosion CoatingsInformation provided by KiON, A Clariant Business.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Liquid
Viscosity 80 cP

@Temperature 19.0 °C
80 cP

@Temperature 66.2 °F
Thermal Properties Metric English Comments
Flash Point 29.0 °C
84.2 °F
Descriptive Properties Value Comments
%Resin 100% solids as liquid
Appearance Clear to pale yellow liquid