Material Notes:
Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and fire point minimize the possibility of fire problems.Stable additive package — Minimal loss of additives due to extended use.Minimal oil carryout — The light viscosity of this oil allows quick drainage from metal parts preventing carryout.Excellent thermal stability — Provides high heat resistance to oxidation and thickening.Deeper, more uniform hardening due to controlled cooling of metals.Texaco Quenchtex oils are highly refined, paraffinic based quenching oils.They provide controlled cooling of steel which is important in steel hardening. When quenching is started, Texaco Quenchtex oils provides a high initial cooling rate inducing maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stresses and metal distortion.Texaco Quenchtex MM is used in quenching and mar-quenching operations and is recommended for the production of very hard parts, especially where distortion of the quenched parts cannot be tolerated.These oils resist the oxidizing effects of quenching and are less sensitive to the effects of agitation. They are highly heat resistant. No additive replacement is required and, in normal service, they retain the original viscosity indefinitely.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.CPS Number: 221508; MSDS Number: 10310
Physical Properties Metric English Comments
API Gravity 28.5 °
28.5 °
Viscosity Measurement 100
100
Viscosity Index
Saybolt Viscosity at 100°F 1149 SUS
1149 SUS
Saybolt Viscosity at 210°F 98 SUS
98 SUS
Kinematic Viscosity at 40°C (104°F) 218 cSt
218 cSt
Kinematic Viscosity at 100°C (212°F) 19.3 cSt
19.3 cSt
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
Flash Point 280 °C
536 °F
310 °C
590 °F
[°C] Fire Point
Descriptive Properties Value Comments
Quench Time, s 32