Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 202 °C | 395 °F | |
Lubriplate APG-90 Petroleum-Based Gear, Bearing, & Recirculating Oil These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil.. |
|||
Flash Point | 202 °C | 395 °F | |
Lubriplate FB 150 USP Mineral Oil-Based Food Machinery Grade Oil These clear, tacky, adhesive Class H-1 oils resist heavy water washdown and steam. For helical gearboxes, chains, linkages, cams, and slides and wherever a dripless, adhesive fluid lubricant is desi.. |
|||
Flash Point | 202 °C | 396 °F | ASTM D92 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Flash Point | 202 °C | 396 °F | |
ELM® 80W90 Multi-Purpose Biodegradable – Biobased Gear Lubricant Description: ELM 80W90 Multi-Purpose Gear Lubricant is a premium quality biodegradable gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the .. |
|||
Flash Point | 202 °C | 396 °F | ASTM D92 |
ChevronTexaco ISO 150 Saw Guide Oil FeaturesChevron Saw Guide Oil is manufactured using naphthenic oils and specially selected additives
balanced to reduce friction between saw and guide components in thin kerf saw equipment. These ad.. |
|||
Flash Point | 202 °C | 396 °F | ASTM D92 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Flash Point | 202 °C | 395 °F | |
ConocoPhillips Sulnap® 22 Cutting Oil Description: Conoco Sulnap Cutting Oil is suited for general-purpose machining operations, such as turning, boring, planing, shaping, light- to medium-duty threading, sawing, hobbing and gear cuttin.. |
|||
Flash Point | 202 °C | 396 °F | ASTM D92 |
ChevronTexaco DEXRON®-III/MERCON® Automatic Transmission Fluid General DescriptionDEXRON® is a specification for General Motors vehicles, but many foreign manufactures specify a DEXRON approved ATF as well. DEXRON-III can be used in transmissions that call for.. |
|||
Flash Point | 202 °C | 396 °F | ASTM D92 |
ChevronTexaco Superla® 18 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Flash Point | 202 °C | 395 °F | |
ConocoPhillips Hydroclear® 115 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Flash Point | 202 °C | 396 °F | |
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid Havoline Automatic Transmission Fluid MERCON/DEXRON-III delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excel.. |