ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Havoline®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Havoline Automatic Transmission Fluid MERCON/DEXRON-III delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excellent base oil and extra oxidation inhibitors.Quiet Performance, especially effective in reducing transmission "chatter". Fast circulation during cold weather and excellent lubricating body when hot.Havoline Automatic Transmission Fluid MERCON/DEXRON-III is the latest high performance, multipurpose, pwer transmission fluit approved under Mercon® and Dexron® specifications. It is developed for passenger car and light truck automatic transmissions.It is manufactured from select Group II base oils and additives that provide oxidation and thermal stability, friction control, load-carrying ability, corrosion and wear protection. It prevents the accumulation of deposits and the formation of sludge, varnish, and foam.Under the most severe operating conditions, Havoline Automatic Transmission Fluid MERCON/DEXRON-III:Maintains friction control for smooth shift actionIs specially formulated to prevent shudderRetains low temperature fluidity and high temperature stability for long operating periods.Protects automatic transmission fluid coolers from corrosion.Practically eliminates transmission overhauls due to sludge, corrosion, wear of clutches and bands, gears and bearings, leakage past seals, and loss of frictional properties.Havoline Automatic Transmission Fluid MERCON/DEXRON-III is designed for use in General Motors Corporation transmissions that require a DEXRON-II, DEXRON-II or DEXRON-IIE fluid, and Ford Motor Company transmissions that require a MERCON fluid. It is also used as a light oil in compressors, pumps and hydraulic systems.Always check your owners manual to determine the proper automatic transmission fluid for your transmission.Ford transmissions manufactured after 1996 may require a MERCON V.Chrysler transmissions manufactured after 1996 require either ATF+3® or ATF+4®3.Havoline Automatic Transmission Fluid MERCON V meets or exceeds:Manufacturers performance requirementsFord MERCONGeneral Motors DEXRON-IIIAllison C4Caterpillar TO-2Denison P-46 Piston PumpVickers PumpVoith DIWA TransmissionsAF transmissionsTypical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221854; MSDS Number: 8654
Physical Properties Metric English Comments
API Gravity 32.7 °
32.7 °
Brookfield Viscosity 17000 cP

@Temperature -40.0 °C
17000 cP

@Temperature -40.0 °F
Viscosity Measurement 172
172
Viscosity Index
Saybolt Viscosity at 100°F 180 SUS
180 SUS
Saybolt Viscosity at 210°F 50.3 SUS
50.3 SUS
Kinematic Viscosity at 40°C (104°F) 35.5 cSt
35.5 cSt
Kinematic Viscosity at 100°C (212°F) 7.2 cSt
7.2 cSt
Thermal Properties Metric English Comments
Pour Point -48.0 °C
-54.4 °F
Flash Point 202 °C
396 °F
Descriptive Properties Value Comments
Color Red