Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 202 °C | 395 °F | |
Lubriplate APG-90 Petroleum-Based Gear, Bearing, & Recirculating Oil These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil.. |
|||
Flash Point | 202 °C | 395 °F | |
Lubriplate FB 150 USP Mineral Oil-Based Food Machinery Grade Oil These clear, tacky, adhesive Class H-1 oils resist heavy water washdown and steam. For helical gearboxes, chains, linkages, cams, and slides and wherever a dripless, adhesive fluid lubricant is desi.. |
|||
Flash Point | 202 °C | 395 °F | |
ConocoPhillips Sulnap® 22 Cutting Oil Description: Conoco Sulnap Cutting Oil is suited for general-purpose machining operations, such as turning, boring, planing, shaping, light- to medium-duty threading, sawing, hobbing and gear cuttin.. |
|||
Flash Point | 202 °C | 395 °F | |
ConocoPhillips Hydroclear® 115 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |