Polymer Property : Flash Point = 125 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 125 °C
257 °F
Tested according to Directive 92/69/EEC
Solvay Chemicals F1EC Monofluoroethylene carbonate
Monofluoroethylene carbonate is applied for the use in batteries and accumulators. 4-fluoro-1,3-dioxolane-2-one: CAS-No.: 114435-02-8Uses: Batteries and accumulators and SolventInformation provided..
Flash Point 125 °C
257 °F
Tested according to Directive 92/69/EEC
Solvay Chemicals Monofluoroethylencarbonate
Fluorinated Solvents for Li-Ion batteries CAS-No.: 114435-02-8 Uses: Batteries and accumulators and SolventInformation provided by Solvay
Flash Point 125 °C
257 °F
ChevronTexaco EDM Fluid
Texaco EDM Fluid delivers value through:Accurate machining — Good dielectric properties provide controlled discharge characteristics. Low viscosity provides excellent fluidity through the spark gap..
Flash Point >= 125 °C
>= 257 °F
A Component; ASTM D92
Aptek 2201-A/B Fast set urethane adhesive
APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f..
Flash Point >= 125 °C
>= 257 °F
B Component; ASTM D92
Aptek 2201-A/B Fast set urethane adhesive
APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f..
Flash Point >= 125 °C
>= 257 °F
B Component; ASTM D92
Aptek 2205 A/B Low modulus urethane stacking compound
APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although..
Flash Point >= 125 °C
>= 257 °F
A Component; ASTM D92
Aptek 6513-A/B Versatile, fast set adhesive
APTEK 6513-A/B is a hazy clear, two component, general purpose, semi-rigid, paste adhesive for bonding to steel, aluminum, wood, concrete, glass, ceramics, bras, and a variety of plastics. It is sp..
Flash Point >= 125 °C
>= 257 °F
B Component; ASTM D92
Aptek 6513-A/B Versatile, fast set adhesive
APTEK 6513-A/B is a hazy clear, two component, general purpose, semi-rigid, paste adhesive for bonding to steel, aluminum, wood, concrete, glass, ceramics, bras, and a variety of plastics. It is sp..
Flash Point >= 125 °C
>= 257 °F
A Component; ASTM D92
Aptek 6516-A/B Electrically conductive epoxy adhesive
General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of..
Flash Point >= 125 °C
>= 257 °F
B Component; ASTM D92
Aptek 6516-A/B Electrically conductive epoxy adhesive
General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of..
Flash Point >= 125 °C
>= 257 °F
A Component; ASTM D92
Aptek 6550-A/B Epoxy Encapsulant
High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for..
Flash Point >= 125 °C
>= 257 °F
B Component; ASTM D92
Aptek 6550-A/B Epoxy Encapsulant
High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for..