Solvay Chemicals F1EC Monofluoroethylene carbonate

Category Fluid , Solvent
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals F1EC Monofluoroethylene carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Monofluoroethylene carbonate is applied for the use in batteries and accumulators. 4-fluoro-1,3-dioxolane-2-one: CAS-No.: 114435-02-8Uses: Batteries and accumulators and SolventInformation provided by Solvay
Thermal Properties Metric English Comments
Melting Point 22.0 °C
71.6 °F
OECD Test Guideline 102
Boiling Point 212 °C
414 °F
Tested according to Directive 92/69/EEC.
Flash Point 125 °C
257 °F
Tested according to Directive 92/69/EEC
Descriptive Properties Value Comments
Appearance wax
Color Colorless
Composition >99%
4-fluoro-1,3-dioxolane-2-one