Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -25.0 °C | -13.0 °F | TCC |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Flash Point | -25.0 °C | -13.0 °F | TCC |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |