Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 72.0 °C | 162 °F | ISO 306 |
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance... |
|||
Softening Point | 72.0 - 88.0 °C | 162 - 190 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 72.0 - 88.0 °C | 162 - 190 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-783 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Softening Point | 72.0 °C | 162 °F | JIS K-2531 |
Unitika elitel UE3380 Polyester, Flake Low molecular weight type UE3200, Low softening point, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products.. |