Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 72.0 - 88.0 °C | 162 - 190 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 72.0 - 88.0 °C | 162 - 190 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-783 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |