Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylac® HF96 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 1.8 MPa (264 psi) 86.7 - 152 °C
188 - 306 °F
Average value: 139 °C Grade Count:85
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
unannealed; ASTM D648
Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS)
High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® ABS LE WT
Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Annealed; ASTM Data
Dow Retain® PS-4000 Polystyrene
Data provided by Dow Chemical.
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
ASTM D648
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene
Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC.
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Techmer ES Statiblend® PP FR BK
Availability: North AmericaForms: PelletsFeature: Flame Retardant, Homopolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.