Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.3 °C | 173 °F | ASTM D648 |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.3 °C | 173 °F | annealed; ASTM D648 |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.3 °C | 173 °F | ASTM D648 |
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.3 °C | 173 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances.. |