Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 75.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 - 75.6 °C
129 - 168 °F
Average value: 67.1 °C Grade Count:12
Overview of materials for PVC, Sheet Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M..