Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 71.7 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Plaskolite Optix® CA - 41 HF General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C

@Thickness 3.18 mm
161 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C

@Thickness 3.18 mm
161 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C

@Thickness 3.18 mm
161 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Plaskolite West Optix® CP - 41 HF General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 4455 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Axiall 8132 Rigid PVC, Extrusion
Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. ..