Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | ASTM D-648 |
Plaskolite Optix® CA - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | ASTM D-648 |
Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C @Thickness 3.18 mm |
161 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C @Thickness 3.18 mm |
161 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C @Thickness 3.18 mm |
161 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | ASTM D-648 |
Plaskolite West Optix® CP - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | ASTM D-648 |
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | Unannealed; ASTM Data |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.7 °C | 161 °F | ASTM D-648 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |