Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 8132 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8132 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. It is widely used for clear profiles such as furniture trim, shower doors, and protected jalousie windows. High impact vacuum formed sheet applications are filled with 8132. Electronic packaging products are specified using this product. Twin screw machines may be used to convert 8132. Georgia Gulf 8132 is characterized by excellent physical properties and easy processing. It contains UV inhibitor to retard deterioration. It is available in fiberboard boxes, railroad bulk hopper cars or bulk truckloads. 8132 is available in a blue tint. It is easily colored by concentrates at the machine.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 2.45 GPa
356 ksi
ASTM D-638
Flexural Strength 78.46 MPa
11380 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 1.33 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
6.67 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 187 kJ/m²
89.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.040 inch(min. thickness)
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D-1003-61
Transmission, Visible 75 %

@Thickness 3.17 mm
75 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F
Descriptive Properties Value Comments
Cell Classification 14444233
ASTM D-4216
Copyright © lookpolymers.com All Rights Reserved