Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 70.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
ASTM D648
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled
Information provided by Niche Polymer
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C

@Thickness 3.18 mm
159 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
ASTM D648
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa..
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
BCC Products BC 5008-2 General Purpose Epoxy System
BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A..
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
annealed; ASTM D-648
Axiall 6511 Rigid PVC, Molding
Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformab..