Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 6511 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 6511 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformabilityExtrudability in Profile and SheetMoldability in Fence CapsInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D-638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.59 GPa
375 ksi
ASTM D-790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
annealed; ASTM D-648
Descriptive Properties Value Comments
Cell Classification 14434323
ASTM D-4216
Flow Ratio (Distance/Wall Thickness, 390-400°F) 160
Internal
Copyright © lookpolymers.com All Rights Reserved