Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
ISO 75-f
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
ASTM D648-45
Manifattura Cattaneo VESPEL® SP1 Polyimide
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
ASTM D648-45
Manifattura Cattaneo VESPEL® SP21 Polyimide
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-C CM Conductive Polyimide Bearing
Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-C DF Conductive Polyimide Bearing
Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-ESD CM Polyimide Bearing
Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G15 CM 15% Graphite Filled Aromatic Polyimide Bearing
Compression Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded ..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G40 CM 40% Graphite Filled Aromatic Polyimide Bearing
Compression Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbo..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-G40 ISO 40% Graphite Filled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 car..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing
Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the ..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing
Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS ..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Deflection Temperature at 1.8 MPa (264 psi) 360 °C
680 °F
Daelim H&L Plavis-ESD DF Polyimide Bearing
Direct Formed. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis info..
Copyright © lookpolymers.com All Rights Reserved