Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | ISO 75-f |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | ASTM D648-45 |
Manifattura Cattaneo VESPEL® SP1 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | ASTM D648-45 |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-C DF Conductive Polyimide Bearing Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-ESD CM Polyimide Bearing Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G15 CM 15% Graphite Filled Aromatic Polyimide Bearing Compression Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G40 CM 40% Graphite Filled Aromatic Polyimide Bearing Compression Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-G40 ISO 40% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 car.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 360 °C | 680 °F | |
Daelim H&L Plavis-ESD DF Polyimide Bearing Direct Formed. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis info.. |