Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 570 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Annealed, 0.125 in bars; ASTM D648
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated  (discon
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed, 0.250 in bars; ASTM D648
PolyOne Lubri-Tech™ PK-30CF/15T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated  (discon
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
LNP Lubricomp® LCL-4033 EM Polyetheretherketone, Carbon Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ASTM D648
Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu..
Deflection Temperature at 1.8 MPa (264 psi) 299 °C
570 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)  (discontinued **)
Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi..