Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Niche Polymer PA66GF13BK Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Niche Polymer PA66GF13N Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PET GF45 X 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 227 °C | 440 °F | ASTM D648 |
Asahi Kasei Thermofil N5-15FG-1103 15% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |