Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil N5-15FG-1103 15% Glass Fiber Reinforced, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 5.93 GPa
860 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
6.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 43.2 µm/m-°C

@Temperature 20.0 °C
24.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 227 °C
440 °F
ASTM D648