Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 171 °C
160 - 340 °F
Average value: 131 °C Grade Count:13
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Deflection Temperature at 1.8 MPa (264 psi) 125 - 171 °C
257 - 340 °F
Average value: 159 °C Grade Count:4
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..