Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 328 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 328 °C
622 °F
ISO 75-f
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Deflection Temperature at 1.8 MPa (264 psi) 328 °C
622 °F
ISO 75-f
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Deflection Temperature at 1.8 MPa (264 psi) 328 °C
622 °F
ISO 75-1/-2
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced
PEEK-GF30Information provided by BARLOG plastics GmbH.