Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Barlog Plastics
Trade Name KEBAPEAK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEEK-GF30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Water Absorption 0.020 %
0.020 %
similar to ISO 62 test
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Modulus 11.8 GPa
1710 ksi
ISO 527-1
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 328 °C
622 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Descriptive Properties Value Comments
Resin Type PEEK-GF30