Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 - 151 °C
183 - 304 °F
Average value: 116 °C Grade Count:16
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Deflection Temperature at 1.8 MPa (264 psi) 122 - 151 °C
252 - 304 °F
Average value: 131 °C Grade Count:16
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 151 °C
140 - 304 °F
Average value: 110 °C Grade Count:21
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..