Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 275 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 - 135 °C
225 - 275 °F
Average value: 114 °C Grade Count:5
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 135 °C
104 - 275 °F
Average value: 67.5 °C Grade Count:6
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..