Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 - 216 °C | 158 - 420 °F | Average value: 186 °C Grade Count:36 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 74.0 - 216 °C | 165 - 420 °F | Average value: 96.5 °C Grade Count:13 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 - 216 °C | 135 - 420 °F | Average value: 98.3 °C Grade Count:29 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 - 216 °C | 178 - 421 °F | Average value: 191 °C Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |