Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C @Thickness 3.18 mm |
135 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP522-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products HP522-390 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, AYCA Medium Prairie Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 TS15 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Silicone Lubricant and PTFE LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 TS18 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP CO FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T30L1 Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 57.2 °C | 135 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced |