Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 155 - 202 °C
311 - 396 °F
Average value: 178 °C Grade Count:21
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 202 °C
170 - 395 °F
Average value: 139 °C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..