Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | Unannealed; ISO 75-2/C |
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | Unannealed; ISO 75-2/C |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40 Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50 Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl.. |
|||
Deflection Temperature at 8.0 MPa | 210 °C | 410 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |