Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 210 °C
410 °F
Unannealed; ISO 75-2/C
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Deflection Temperature at 8.0 MPa 210 °C
410 °F
Unannealed; ISO 75-2/C
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVL-4H nat PA*-GF40
Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40
Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40
Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
Deflection Temperature at 8.0 MPa 210 °C
410 °F
HDT/C; ISO 75-2
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Copyright © lookpolymers.com All Rights Reserved