Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 126 °C | 259 °F | ISO 75-1/-2 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
Deflection Temperature at 8.0 MPa | 126 °C | 259 °F | ISO 75-1/-2 |
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |